View Single Post
Old 01-02-2019, 10:20 AM   #38
Biggd
Senior Member
 
Join Date: Nov 2016
Location: Waltham Ma./Meredith NH
Posts: 4,421
Thanks: 2,428
Thanked 1,270 Times in 813 Posts
Default

You can also use pressure treated boards but you have to let them dry out a month or two before you stain or paint them. I just bought 1" x 8" this past summer and stained it after about a month with a solid oil based Olympic stain. Somehow painting Azek defeats the purpose of using plastic. Once you paint it, it's no longer maintenance free, JMO.

Last edited by Biggd; 01-02-2019 at 11:14 AM.
Biggd is offline   Reply With Quote